Atomic Layer Deposition on Suspended Single-Walled Carbon Nanotubes via Gas-Phase Noncovalent Functionalization
Publication information:
Farmer, Damon, and Roy Gordon. “Atomic Layer Deposition on Suspended Single-Walled Carbon Nanotubes via Gas-Phase Noncovalent Functionalization”. Nano Letters 6, no. 4 (2006): 699-703.