Atomic layer deposition of tin oxide with nitric oxide as an oxidant gas
Publication information:
Heo, Jaeyeong, Sang Bok Kim, and Roy Gordon. “Atomic Layer Deposition of Tin Oxide With Nitric Oxide As an Oxidant Gas”. Journal of Materials Chemistry 22 (2012): 4599-4602.